Ceradyne Ceralloy® 137 CB AlN Composite

Category Ceramic , Nitride
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® 137 CB AlN Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersFeatures: higher thermal conductivity then Ceraloy® BeO-SiC at temperatures greater then 150°C, close match in electrical properties.Information provided by Ceradyne Company
Physical Properties Metric English Comments
Density 2.99 g/cc
0.108 lb/in³
Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 1000 °C
2.78 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 95.0 - 105 W/m-K
659 - 729 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 28

@Frequency 1e+10 Hz
28

@Frequency 1e+10 Hz
30

@Frequency 8.00e+9 Hz
30

@Frequency 8.00e+9 Hz
40

@Frequency 1e+9 Hz
40

@Frequency 1e+9 Hz
Dissipation Factor 0.15

@Frequency 1e+9 Hz
0.15

@Frequency 1e+9 Hz
0.30

@Frequency 8.00e+9 Hz
0.30

@Frequency 8.00e+9 Hz
0.30

@Frequency 1e+10 Hz
0.30

@Frequency 1e+10 Hz