Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CeramTec Sonox® P41 Piezoceramic

Category Ceramic , Oxide , Piezoelectric
Manufacturer CeramTec North America
Trade Name Sonox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CeramTec Sonox® P41 Piezoceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P41 is specifically used to make squeeze igniters.
Electrical Properties Metric English Comments
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 25
25
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 260
260
Descriptive Properties Value Comments
Capacitance (pF) 20
CT-Type 39601
23
CT-Type 39613
Users viewing this material also viewed the following: