Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P8 is designed to withstand high electrical control voltages and intense mechanical (pressure) loads. It features low dielectric loss, dielectric constants between 1000 and 1600, and high Q values (between 500 and 2000). It is well suited for high-performance ultrasonic applications in the 20 kHz to several MHz range. P8 is specifically used for ultrasonic welding and drilling.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 305 °C
581 °F
Tc
Dielectric Constant 540
540
e33 S/e?
800
800
e11 S/e?
1000
1000
e33 T/e?
1250
1250
e11 T/e?
Dissipation Factor 0.0020
0.0020
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.68
0.68
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -95.0
-95.0
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 380
380
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 27.1
27.1
Piezoelectric Planar Coupling Factor, kp 0.55
0.55
Piezoelectric Mechanical Q 1000
1000
Piezoelectric Shear Coupling Factor, k15 0.60
0.60
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 240
240
Piezoelectric Transverse Coupling Factor, k31 0.30
0.30
Descriptive Properties Value Comments
Aging Rates (%/decade) 1
Cf
-1.8
Ce
-2.2
Ck
Elastic Compliance (10^-12 m²/N) 11.4
s11^E
13.7
s33^E
Elastic Rigidity (10^10 N/m²) 16.2
c33^D
Frequency Constants (kHz·mm) 1490
N3
1600
N1
2020
Nt
2280
Np
Piezoelectric Coupling Coefficient, kt 0.48
Piezoelectric Voltage Coefficient, e33 (C/m²) 13.3