Channel Industries 600 Barium Titanate Piezoelectric

Category Ceramic , Oxide , Titanium Oxide , Piezoelectric
Manufacturer Channel Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Channel Industries 600 Barium Titanate Piezoelectric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for use in devices such as depth sounders and expendable hydrophones.Uses of this grade include: Low Power Sonar; Ultrasonic CleanersCoupling Constants:k33: 0.39k31: -0.16k15: 0.39kp: -0.27Piezoelectric Constants:d33: 82 x 10-12 m/Vd31: -33 x 10-12 m/Vd15: 150 x 10-12 m/Vg33: 16.8 x 10-3 Vm/Ng31: -6.8 x 10-3 Vm/Ng15: 29.8 x 10-3 Vm/N.Mechanical Q: 1200Data provided by Channel Industries, Inc.
Physical Properties Metric English Comments
Density >= 5.40 g/cc
>= 0.195 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.0 MPa
3480 psi
Dynamic tensile strength
59.0 MPa
8560 psi
Static
Electrical Properties Metric English Comments
Curie Temperature >= 140 °C
>= 284 °F
Dielectric Constant 570
570
K<sup>T</sup><sub>1</sub>
625
625
Free dielectric constant K<sup>T</sup><sub>3</sub>
Dissipation Factor 0.0030
0.0030
Low Field
Piezoelectric Longitudinal Coupling Factor, k33 0.39
0.39
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -33.0
-33.0
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 150
150
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 16.8
16.8
Piezoelectric Planar Coupling Factor, kp -0.270
-0.270
Piezoelectric Mechanical Q 1200
1200
Piezoelectric Shear Coupling Factor, k15 0.39
0.39
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 82
82
Piezoelectric Transverse Voltage Coefficient, g31, 10^-3 V-m/N -6.80
-6.80
Piezoelectric Shear Voltage Coefficient, g15, 10^-3 V-m/N 29.8
29.8
Piezoelectric Transverse Coupling Factor, k31 -0.160
-0.160