Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® N100MD2 (DAM) Nylon 6 with 2% MoS2 Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
380 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648