Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic E500G10 PC/PET, 10% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend, Glass Reinforced , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic E500G10 PC/PET, 10% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Index of Compound 16 g/10 min
16 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength, Yield 76.5 MPa
11100 psi
ASTM D638
Flexural Modulus 5.00 GPa
725 ksi
ASTM D790
Izod Impact, Notched 7.85 J/cm
14.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved