Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic FV30725 POM, 25% Mineral Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Mineral Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic FV30725 POM, 25% Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
ASTM D785
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Flexural Yield Strength 162 MPa
23500 psi
ASTM D790
Izod Impact, Notched 0.343 J/cm
0.643 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
ASTM D648
Flammability, UL94 HB
HB