Description: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The product deposits a 95% pure zinc coating that bonds to metal protecting it against corrosion both physically and by galvanic action. After fabrication or construction, it forms an all purpose protective coating. After wear, accidents, welding or maintenance work on galvanized protective coating. Chesterton 752 Cold Galvanizing Compound provides instant galvanizing. Unlike hot dip galvanizing, the product can be sprayed on to provide a convenient, fast drying protective coating.Features:95% pure zinc in dried filmUltra-fine particle sizeFlexibleNo heat requiredFast dryingSelf healingOne part system3 way corrosion protectionConforms to MIL-P-46105, MIL-P-21035 and MIL-P-26915Authorized by the USDAApplications: Use in maintenance and construction to restore damaged galvanized metal dn provide protection for all iron and steel surfaces, structures or equipment such as air conditioning units, agricultural machinery, automotive bodies, fences, marine equipment, metal floors and roofs, mining equipment and oil rigs, off shore drilling structures, ornamental iron works, pipe lines, railroad equipment, structural steel tanks, transmission towers, underground pipe lines, welds, ducts, marine equipment, decks etc.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 2.88 g/cc
2.88 g/cc
Mechanical Properties Metric English Comments
Impact Test 4.52 J
3.33 ft-lb
Extrusion; ASTM D2794
>= 9.04 J
>= 6.67 ft-lb
Intrusion; ASTM D2794
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Application Temperature
149 °C
300 °F
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Application Temperature
Processing Properties Metric English Comments
Dry Time 0.250 hour

@Temperature 21.0 °C
0.250 hour

@Temperature 69.8 °F
Touch
8.00 hour

@Temperature 21.0 °C
8.00 hour

@Temperature 69.8 °F
Recoat
Descriptive Properties Value Comments
Color Gray
Corrosion Protection: 2500 hrs
ASTM B117
Coverage 6.6-9.8 m2/l
at 0.05-0.08
Diluent Xylol
Zinc Content (Dried Film) 0.95