Material Notes:
Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.Determined on mineral oil extracted by vacuum filtration.CPS Number: 222314; MSDS Number: 9001
Physical Properties Metric English Comments
Solids Content 12 %
12 %
Viscosity Measurement 72
72
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 394 SUS
394 SUS
See Note 3.
Saybolt Viscosity at 210°F 54 SUS
54 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 75.3 cSt
75.3 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 8.4 cSt
8.4 cSt
See Note 3.
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 340
340
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 78.0 °C
172 °F
See Note 2.
Minimum Service Temperature, Air -23.0 °C
-9.40 °F
See Note 1.
Flash Point 172 °C
342 °F
See Note 3.
Dropping Point 99.0 °C
210 °F
Descriptive Properties Value Comments
Color Black
Texture Smooth
Thickener, % 10
Calcium