ChevronTexaco Cleartex® CF F

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Cleartex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Cleartex® CF F.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Cleartex CF metalworking fluid delivers value through:Multipurpose performance — Texaco Cleartex CF metalworking fluid is tri-purpose - serving as the cutting oil, hydraulic fluid, and machine lubricant in machine tools - eliminates the problem of machine lubricants contaminating the cutting oil, and allows the end-user to minimize inventories of other lubricants.Chlorine-free EP compounding provides benefits in the areas of storage and waste disposal without sacrificing cutting oil performance.Antimist control minimizes the amount of stray mist around the machine, improving shop cleanliness and reducing operator exposure.Texaco Cleartex CF metalworking fluid is transparent, light colored, chlorine-free metalworking fluids.Texaco Cleartex CF metalworking fluid is formulated with naturally high viscosity index paraffinic base stocks.This metalworking fluid has a high flash point, minimizing the potential for fire.The EP compounding in Texaco Cleartex CF metalworking fluid is nonstaining to yellow metals, provides long tool life, and allows for faster machine rates.The chlorine-free nature of this metalworking fluid addresses many of the issues associated with chlorinated metalworking fluids, such as storage and waste disposal or staining of certain aluminum alloys.Texaco Cleartex CF metalworking fluid can be used as the cutting oil, hydraulic oil, and machine lubricant in automatic screw machines. This eliminates the contamination problem caused by leakage of these fluids into the cutting oil, reducing cutting oil effectiveness.Texaco Cleartex CF metalworking fluid is effective at providing rust and corrosion protection of parts, cutting tools, and the machine.Texaco Cleartex CF metalworking fluid:provides excellent cooling and lubrication in a wide range of machining operationsprevents welding of chip and toolflushes chips away from the work areaprotects the finished work surfaces, tools, and machines against rusting and stainingreduces oil mist in high speed machine toolsTexaco Cleartex CF F is recommended for:general purpose machining where the service ranges from light to moderately severemachining operations on free-machining to intermediate steels and difficult to machine nonferrous metals as well as more difficult metals, such as stainless steelTexaco Cleartex CF metalworking fluid is widely used in automatic screw machines and NC/CNC machining centers.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.CPS Number: 220741; MSDS Number: 8967
Physical Properties Metric English Comments
API Gravity 31.3 °
31.3 °
Saybolt Viscosity at 100°F 172 SUS
172 SUS
Saybolt Viscosity at 210°F 47 SUS
47 SUS
Kinematic Viscosity at 40°C (104°F) 36.7 cSt
36.7 cSt
Kinematic Viscosity at 100°C (212°F) 6.3 cSt
6.3 cSt
ASTM Color 3.5
3.5
ASTM D1500
Thermal Properties Metric English Comments
Flash Point 226 °C
439 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Calcium Present
Chlorine None
Fatty Oil Present
Sulfur Present