ChevronTexaco Delo® 400 Synthetic, SAE 5W-40

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Delo®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Delo® 400 Synthetic, SAE 5W-40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chevron Delo 400 Synthetic heavy duty motor oils are multipurpose 100% synthetic lubricants formulated for use in gasoline and diesel engines, torque converters, gear cases, and hydraulic systems operating in subzero arctic-type temperatures. They are manufactured using stable synthetic base stocks. These oils utilize highly dispersed viscosity index improvers that promote stable viscosities and soot dispersancy between oil drains.Applications:Chevron Delo 400 Synthetic heavy duty motor oils are recommended fro use in diesel and four-stroke cycle gasoline engines, torque converters, gear cases, and hydrualic systems oeprating year-round in arctic-type climates. They utilize the latest technology to provide excellent performance with either high or low sulfur diesel fuels.Chevron Delo 400 Synthetic heavy duty motor oils meet:API Service Categories: CG-4, CF, CD, SH, SJ, Energy Conserving for API SH (SAE 0W-30), CI-4(SAE 5W-40)Major diesel engine manufacturers requirements: Mack EO-M PLUS, EO-M (SAE 5W-40), Cummins CES 20076, 20071 (SAE 5W-40)Performance requirements of: Allison C4 (SAE 0W-30)Manufacturers performance requirements: Ford ESE-M2C153-E, General Motors GM 6094-M
Physical Properties Metric English Comments
API Gravity 31.5 °
31.5 °
Viscosity 3150 cP

@Temperature -25.0 °C
3150 cP

@Temperature -13.0 °F
Cold Crank
Viscosity Measurement 175
175
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 94.5 cSt
94.5 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 15.6 cSt
15.6 cSt
ASTM D445
Ash 1.5 %
1.5 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -43.0 °C
-45.4 °F
ASTM D97
Flash Point 232 °C
450 °F
ASTM D92
Component Elements Properties Metric English Comments
Phosphorous, P 0.136 %
0.136 %
Zinc, Zn 0.151 %
0.151 %
Chemical Properties Metric English Comments
Total Base Number 12.5
12.5
ASTM D2896