Material Notes:
Texaco Metal Protective Oil L delivers value through:Excellent short-term rust protection — After evaporation of the solvent, a highly protective, nondrying oil film remains which provides a higher level of protection against corrosion than lower viscosity products. The corrosion inhibitors in the oil resist chemical attack by water, other fluids and particulate matter.Minimum drippage — Viscosity of the oil is low enough to enable ready drain-off of excess oil. High volatility of the solvent ensures rapid evaporation, minimizing post-application dripping.Easy removal — Oil film is readily soluble in petroleum solvent or kerosene to enable easy removal when required.Texaco Metal Protective Oil L is a higher viscosity, rust protective oil designed for the temporary rust protection of steel in covered storage or packaged shipment.It contains corrosion inhibitors and is diluted with a petroleum solvent for ease of application.Texaco Metal Protective Oil L is recommended for:Use as temporary protection of plain and galvanized steel sheet, coils, bars, rods and tubes during undercover storage, protected shipment or interprocess handlingProtection against yellow-line stain that tends to form on stacked sheets or coiled strip; white rust on galvanized steel; red rustMay be applied by brush, roller, dip, or spray.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221052; MSDS Number: 10690
Physical Properties Metric English Comments
API Gravity 27.1 °
27.1 °
Saybolt Viscosity at 100°F 92 SUS
92 SUS
Kinematic Viscosity at 40°C (104°F) 17 cSt
17 cSt
Thermal Properties Metric English Comments
Pour Point -23.0 °C
-9.40 °F
Flash Point 88.0 °C
190 °F