China Tungsten YG4C Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG4C Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 3.40 g/cc
0.123 lb/in³
Density 15.15 g/cc
0.5473 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92.5
92.5
Tensile Strength, Ultimate 2300 MPa
334000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 4.0 %
4.0 %
WC 96 %
96 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 21-25