China Tungsten YG8 Tungsten Carbide for Cutting Tools

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG8 Tungsten Carbide for Cutting Tools.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength in use ,impact and shock resistance higher than YG6,but wear resistance and cutting speed comparatively lower. Roughing of cast irons non ferrous metals and their alloys as well as nonmetallic  materials at low cutting speedInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 14.7 g/cc
0.531 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 90
90
Flexural Strength 2520 MPa
365000 psi