Material Notes:
Higher wear resistance, service strength and impact toughness than YG6 and YG8. For drawing of steel
Physical Properties Metric English Comments
Density 14.6 - 14.9 g/cc
0.527 - 0.538 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A >= 89.5
>= 89.5
Flexural Strength >= 1650 MPa
>= 239000 psi