China Tungsten YMo55.0-A MoO3, Lump Standard

Category Ceramic , Oxide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YMo55.0-A MoO3, Lump Standard.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Antimony, Sb <= 0.040 %
<= 0.040 %
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu <= 0.25 %
<= 0.25 %
Molybdenum, Mo >= 55 %
>= 55 %
Sulfur, S 0.10 - 0.15 %
0.10 - 0.15 %
Tin, Sn <= 0.050 %
<= 0.050 %
Yttrium, Y <= 44.31 %
<= 44.31 %