Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.00 g/cc
0.108 lb/in³
Porosity 3.0 %
3.0 %
Mechanical Properties Metric English Comments
Compressive Strength 40.0 MPa
5800 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Carbon, C 12 %
12 %
MgO 80 %
80 %
Descriptive Properties Value Comments