Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom

Category Ceramic , Oxide , Aluminum Oxide , Magnesium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.00 g/cc
0.108 lb/in³
Porosity 5.0 %
5.0 %
Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 68 %
68 %
Carbon, C 9.0 %
9.0 %
MgO 12 %
12 %