Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0044145 GPa

@Temperature 110 °C,
Time 86400 sec
0.64028 ksi

@Temperature 230 °F,
Time 24.0 hour
0.005886 GPa

@Temperature 500 °C,
Time 10800 sec
0.8537 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 11.8 MPa

@Temperature 110 °C,
Time 86400 sec
1710 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
24.5 MPa

@Temperature 500 °C,
Time 10800 sec
3560 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 800 °C
1470 °F
limited
Shrinkage -0.300 %

@Temperature 500 °C,
Time 10800 sec
-0.300 %

@Temperature 932 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 30 %
30 %
SiO2 65 %
65 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Main Applications Chemical Plant
Material Required for Estimating (kg/?) 1,900
Water Required for Casting(%) 15