Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0024525 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0053955 GPa

@Temperature 500 °C,
Time 10800 sec
0.78256 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 6.86 MPa

@Temperature 110 °C,
Time 86400 sec
996 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
19.6 MPa

@Temperature 500 °C,
Time 10800 sec
2840 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 800 °C
1470 °F
limited
Shrinkage -0.500 %

@Temperature 500 °C,
Time 10800 sec
-0.500 %

@Temperature 932 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 27 %
27 %
SiO2 68 %
68 %
Descriptive Properties Value Comments
Installation Method Spray
Main Applications Chemical Plant
Material Required for Estimating (kg/?) 2,100