Chosun Refractories CO-210 Blast Furnace Runner Refractory

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CO-210 Blast Furnace Runner Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 1.67 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0603 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.06 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0744 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Compressive Strength 5.20 MPa

@Temperature 1500 °C,
Time 10800 sec
754 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
10.5 MPa

@Temperature 110 °C,
Time 86400 sec
1520 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -5.50 %

@Temperature 1500 °C,
Time 7200 sec
-5.50 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 25 %
25 %
SiO2 47 %
47 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 18
Installation Method Ramming
Main Applications Slag runner
Material Required for Estimating (kg/?) 2,100