Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0024525 GPa

@Temperature 1350 °C,
Time 10800 sec
0.35571 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.0024525 - 0.0063765 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 - 0.92485 ksi

@Temperature 230 °F,
Time 24.0 hour
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
14.7 MPa

@Temperature 1350 °C,
Time 10800 sec
2130 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.60484 W/m-K

@Temperature 260 °C
4.1908 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.66300 W/m-K

@Temperature 540 °C
4.5938 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.7560 W/m-K

@Temperature 800 °C
5.238 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
limited
Shrinkage -0.600 %

@Temperature 1500 °C,
Time 10800 sec
-0.600 %

@Temperature 2730 °F,
Time 3.00 hour
-0.120 %

@Temperature 110 °C,
Time 86400 sec
-0.120 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
SiO2 60 %
60 %
Descriptive Properties Value Comments
Installation Method Casting, Troweling
Material Required for Estimating(kg/?) 1,800
Water Required for Casting(%) 14.0