Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Compressive Strength 41.2 MPa

@Temperature 110 °C,
Time 86400 sec
5970 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
82.4 MPa

@Temperature 1500 °C,
Time 10800 sec
11900 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
0.60 %

@Temperature 1500 °C,
Time 10800 sec
0.60 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 91 %
91 %
MgO 6.0 %
6.0 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Main Applications Bottom Wall Rapidfire heating
Material Required for Estimating (kg/?) 3,000
Water Required for Casting(%) 6