Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories FRS 80 Flame-Gunning Repair Refractory

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories FRS 80 Flame-Gunning Repair Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 1.47 g/cc
0.0531 lb/in³
Apparent Bulk Density 2.02 g/cc
0.0730 lb/in³
Porosity 27.05 %
27.05 %
Grain Size <= 700 µm
<= 700 µm
Mechanical Properties Metric English Comments
Compressive Strength 39.2 MPa
5690 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 5.44 %
5.44 %
CaO 2.48 %
2.48 %
Fe2O3 0.52 %
0.52 %
Silicon, Si 9.15 %
9.15 %
SiO2 80.81 %
80.81 %
Descriptive Properties Value Comments
High adhesiveness 90
Main Applications Coke Oven & Glass Melting Tanks
Refractoriness(?) 1,640