Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.01 g/cc
0.0726 lb/in³
Apparent Bulk Density 2.26 g/cc
0.0816 lb/in³
Porosity 11.83 %
11.83 %
Grain Size <= 200 µm
<= 200 µm
Mechanical Properties Metric English Comments
Compressive Strength 49.0 MPa
7110 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 0.65 %
0.65 %
CaO 1.25 %
1.25 %
Fe2O3 0.18 %
0.18 %
Na2O 0.78 %
0.78 %
SiO2 96.56 %
96.56 %
Descriptive Properties Value Comments
High adhesiveness 90
Main Applications Coke Oven
Refractoriness(?) 1,690