Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.25 g/cc
0.0813 lb/in³
Porosity 19 %
19 %
Mechanical Properties Metric English Comments
Compressive Strength 39.2 MPa
5690 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.60 µm/m-°C

@Temperature 1000 °C
3.11 µin/in-°F

@Temperature 1830 °F
Shrinkage -0.500 - 0.50 %

@Temperature 1400 °C,
Time 7200 sec
-0.500 - 0.50 %

@Temperature 2550 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Fe2O3 1.9 %
1.9 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,370
Refractoriness (SK) 34=