Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.01128 GPa

@Temperature 110 °C,
Time 86400 sec
1.636 ksi

@Temperature 230 °F,
Time 24.0 hour
0.01619 GPa

@Temperature 1350 °C,
Time 10800 sec
2.348 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.017658 GPa

@Temperature 1500 °C,
Time 10800 sec
2.5611 ksi

@Temperature 2730 °F,
Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.630 %

@Temperature 1350 °C,
Time 10800 sec
-0.630 %

@Temperature 2460 °F,
Time 3.00 hour
-0.400 %

@Temperature 110 °C,
Time 86400 sec
-0.400 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
MgO 4.5 %
4.5 %
Descriptive Properties Value Comments
Installation Method Troweling
Material Required for Estimating (kg/?) 2,800
Water Required for Casting(%) 7.5