Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.59 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0936 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.63 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0950 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Porosity 17.6 %

@Temperature 110 °C,
Time 86400 sec
17.6 %

@Temperature 230 °F,
Time 24.0 hour
22 %

@Temperature 1500 °C,
Time 10800 sec
22 %

@Temperature 2730 °F,
Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0027468 GPa

@Temperature 110 °C,
Time 86400 sec
0.39840 ksi

@Temperature 230 °F,
Time 24.0 hour
0.01059 GPa

@Temperature 1500 °C,
Time 10800 sec
1.537 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 9.71 MPa

@Temperature 110 °C,
Time 86400 sec
1410 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
29.7 MPa

@Temperature 1500 °C,
Time 10800 sec
4310 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.0600 %

@Temperature 1500 °C,
Time 7200 sec
-0.0600 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
SiC 50 %
50 %
SiO2 3.0 %
3.0 %
Descriptive Properties Value Comments
Chemical Analysis(%),FC 2.8
Installation Method Casing Vibrating
Main Applications Main runner Metal Zone
Material Required for Estimating (kg/?) 2,570
Water Required for Casting(%) 6.2