Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Compuestos Dominicanos Polycom CE-553165 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Compuestos Dominicanos, S.A. (polycom)
Trade Name Polycom
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Compuestos Dominicanos Polycom CE-553165 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resistance and low temperature applications. Products in different colors, hardness, and finish are available for any specific need. Compuestos Dominicanos SA also manufactures specialty compounds that offer high resistance to abrasion for shoe soles.Applications: Expandable shoe soles Appearance: Black PelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.17 - 1.21 g/cc
1.17 - 1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D412
Elongation at Break 320 %
320 %
ASTM D412