Compuestos Dominicanos Polycom PW-103099 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Compuestos Dominicanos, S.A. (polycom)
Trade Name Polycom
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Compuestos Dominicanos Polycom PW-103099 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compuestos Dominicanos' rigid PVC compounds for the extrusion of pipes have excellent processing characteristics and are available in the form of pellets and dry-blend. Also available are compounds for the injection molding of pipefitting, that have outstanding characteristics flow and impact resistance, being suitable for the production of both drainage and pressure fittings and accessories. The polycom PW series are compounds for the extrusion of window profiles, yielding profiles with superior gloss, color uniformity and impact resistance. Applications: Rigid profiles Appearance: White pelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.3 MPa
7300 psi
ASTM D412
Izod Impact, Unnotched 0.500 J/cm
0.937 ft-lb/in
ASTM D256-93
Users viewing this material also viewed the following: