ConocoPhillips 80W-90 Universal Gear Lubricant

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 80W-90 Universal Gear Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Universal Gear Lubricant is an excellent multipurpose, extreme pressure lubricant for differentials and manual transmissions of passenger cars, trucks, vans, buses and off-road equipment that operates under mild to severe service conditions. It is available in two viscosity grades: SAE 80W-90 and SAE 85W-140. Both grades are qualified for API Service GL-5 and MT-1. They meet U.S. Military Specification Mil PRF- 2105E and Mack GO-J. Universal Gear Lubricant can be used in limited-slip differentials for top-off applications. For the complete drain and refill of automotive limited-slip differentials, a special additive is available through local automobile dealerships. Universal Gear Lubricant offers thermal and oxidative stability, as well as maximum protection against gear wear, rust and corrosion. It is also suited for industrial gear drives that call for a AGMA No. 4 or 7 lubricant.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 27 °
27 °
Viscosity Measurement 99
99
Viscosity Index
Saybolt Viscosity at 100°F 700 SUS
700 SUS
Saybolt Viscosity at 210°F 70 SUS
70 SUS
Kinematic Viscosity at 40°C (104°F) 145 cSt
145 cSt
Kinematic Viscosity at 100°C (212°F) 14.8 cSt
14.8 cSt
ASTM Color 7.5
7.5
Thermal Properties Metric English Comments
Pour Point -27.2 °C
-17.0 °F
Flash Point 210 °C
410 °F