ConocoPhillips 90 Transmission Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 90 Transmission Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Transmission Oil 90 is designed for heavy-duty, multiple-speed manual transmissions typically used in on-road trucks and buses, such as Fuller, Clark, Spicer and New Process. It also can be used in other transmissions that call for an API GL-1 mineral oil. Transmission Oil 90 gear lubricant inhibits rust and oxidation; protects gears, bearings and synchronizers; and controls seal swell. It resists foaming to better protect transmissions. Note: Transmission Oil 90 is not recommended for the hypoid gear sets typically found in automotive and truck rear axles. For this application, use an EP gear oil such as Conoco Universal Gear Lubricant SAE 80W-90.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 29.7 °
29.7 °
Viscosity Measurement 97
97
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 149 cSt
149 cSt
Kinematic Viscosity at 100°C (212°F) 14.6 cSt
14.6 cSt
ASTM Color 2.5
2.5
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 277 °C
530 °F