ConocoPhillips Hydroclear® El Mar® Ashless Heavy Duty SAE 40

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear® El Mar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® El Mar® Ashless Heavy Duty SAE 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy Duty is specially formulated with proprietary additive chemistry to meet the requirements of less severe, naturally aspirated and turbocharged, two-cycle gas engines. Hydroclear El Mar Ashless Heavy Duty has demonstrated successful performance results in two-cycle engines manufactured by the following companies: Clark, Cooper Bessemer, Worthington (two-cycle)Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.881 g/cc
0.0318 lb/in³
Viscosity Measurement 100
100
Viscosity Index
Saybolt Viscosity at 100°F 654 SUS
654 SUS
Saybolt Viscosity at 210°F 73 SUS
73 SUS
Kinematic Viscosity at 40°C (104°F) 125 cSt
125 cSt
Kinematic Viscosity at 100°C (212°F) 13.4 cSt
13.4 cSt
Ash 0.0030 %
0.0030 %
Sulfated Ash
ASTM Color 1.5
1.5
Thermal Properties Metric English Comments
Pour Point -33.9 °C
-29.0 °F
Flash Point 266 °C
510 °F
Chemical Properties Metric English Comments
Total Acid Number 0.57
0.57
ASTM D974
Total Base Number 1.5
1.5
Descriptive Properties Value Comments
Carbon Residue 0.07 wt. %