ConocoPhillips Hydroclear® Heat Transfer Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® Heat Transfer Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear Heat Transfer Oil is a high-quality, thermally stable inhibited oil formulated from premium Conoco hydrocracked base stocks for use in heat-transfer service. Hydroclear Heat Transfer Oil is specially formulated with proprietary additive chemistry and is recommended for use in closed liquid-phase heat-transfer systems equipped with expansion tanks and pressure relief valves where the maximum bulk oil temperature does not exceed 550°F. Hydroclear Heat Transfer Oil is also recommended for use in open heat-transfer systems equipped with cold oilsealed expansion tanks where the maximum bulk oil temperature does not exceed 380°F. Typical applications include direct- and indirect-fired asphalt heaters, building heaters, plastic and wax coating equipment and other hot oil systems. Hydroclear Heat Transfer Oil is not recommended for use in vapor-phase heat-transfer systems. Mixing of Hydroclear Heat Transfer Oil with other nonpetroleum-based products is also not recommended. The use of a positive pressure inert gas, such as nitrogen, is recommended at all times on the expansion tank during operation, and measures should be taken to not allow the hot oil to come in contact with air.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.854 g/cc
0.0309 lb/in³
Viscosity Measurement 110
110
Viscosity Index
Saybolt Viscosity at 100°F 160 SUS
160 SUS
Saybolt Viscosity at 210°F 44 SUS
44 SUS
Kinematic Viscosity at 40°C (104°F) 31 cSt
31 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
5.4 cSt
Vapor Pressure 0.0107 bar

@Temperature 260 °C
8.03 torr

@Temperature 500 °F
8 mm Hg
ASTM Color 2.0
2.0
Thermal Properties Metric English Comments
Specific Heat Capacity 1.80 J/g-°C

@Temperature -17.8 °C
0.430 BTU/lb-°F

@Temperature 0.000 °F
2.22 J/g-°C

@Temperature 93.3 °C
0.530 BTU/lb-°F

@Temperature 200 °F
2.59 J/g-°C

@Temperature 204 °C
0.620 BTU/lb-°F

@Temperature 400 °F
2.93 J/g-°C

@Temperature 288 °C
0.700 BTU/lb-°F

@Temperature 550 °F
Pour Point -37.2 °C
-35.0 °F
Flash Point 218 °C
425 °F
Descriptive Properties Value Comments
Autoignition Temperature 680°F
Carbon Residue 0.17 wt.%
Copper Corrosion 1A
Fire point 480°F