Material Notes:
Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recommended for use as a chassis grease for heavy mobile equipment. It is formulated to provide long service life in severe service applications. Tacna HD is manufactured with high-quality, high-viscosity base oils and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives, rust and oxidation inhibitors, and a tackiness additive. It has excellent oxidation resistance, high load-carrying capacity for excellent wear protection, and protects metal parts against rust and corrosion. It has excellent adhesion to bearing surfaces for improved retention and resistance to water washout, and has excellent resistance to structural breakdown even under severe operating conditions.Applications: Heavily loaded plain and rolling-element bearings in industrial and off-road equipment Chassis parts on heavy mobile equipment Construction equipment Dredging equipment Marine deck equipment Offshore drilling equipment Rock quarry equipmentFeatures/Benefits:High load-carrying capacityExcellent shock-load resistanceExcellent oxidation resistanceAdhesive to metal surfacesHigh shear stabilityProtects against rust and corrosionExcellent resistance to water washoutInformation provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.857 g/cc
0.0310 lb/in³
Viscosity Measurement 87
87
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 2150 SUS
2150 SUS
Base Oil Property
Saybolt Viscosity at 210°F 129 SUS
129 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 400 cSt
400 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 26 cSt
26 cSt
Base Oil
Oxidative Stability 100 hour

@Pressure 0.304 MPa
100 hour

@Pressure 44.1 psi
Pressure Drop; ASTM D942
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
ASTM D2596
Four Ball Wear 0.450 mm
0.0177 in
Scar Wear; ASTM D2266
Penetration P(60), 1/10 mm 265 - 295
265 - 295
ASTM D217
Timken Test 24900 g
55.0 lb
ASTM D2509
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -12.0 °C
10.4 °F
Dropping Point >= 260 °C
>= 500 °F
Descriptive Properties Value Comments
Color Red
Copper Corrosion 1b
ASTM D4048
Rust Test A&B Pass
Soap Type (Thickener) Lithium Complex
Texture Smooth/Tacky
Water Washout 2%
ASTM D-1264, @ 175°F