Cotronics Duralco™ 134 500°F (260°C) Aluminum Filled Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Thermally Conductive
Manufacturer Cotronics
Trade Name Duralco™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Duralco™ 134 500°F (260°C) Aluminum Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermally conductive grease provides a non-hardening, electrically insulating and thermally conductive layer between components and heat sinks. Ceramic fillers provide high thermal conductivity along with high dielectric strength. Duralco™ 134 retains its consistency, even after long periods, allowing parts to be easily removed and replaced.
Thermal Properties Metric English Comments
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm