Mechanical Properties Metric English Comments
Flexural Strength 10.3 MPa
1500 psi
Compressive Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
CTE, linear 7.38 µm/m-°C

@Temperature 20.0 °C
4.10 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 8.65 W/m-K
60.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 2980 °C
5400 °F