Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® DP 8798A S043 Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8798A S043 Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
3s; ISO 868
Hardness, Shore D 53
53
15s; ISO 868
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-1/-2
Tensile Strength, Yield 65.0 MPa
9430 psi
parallel; ISO 527-3
17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ISO 527-1/-2
39.0 MPa

@Strain 300 %
5660 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 15
15
mm³; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 815
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
ISO 815