Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, Dry As Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Cresset Powers, Ltd
Trade Name Cress-Alon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, Dry As Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surpasses super tough neat resins in strength, heat resistance, and hardness.Information provided by Cresset Powers Ltd.
Physical Properties Metric English Comments
Density 1.064 g/cc
0.03844 lb/in³
ASTM D792
Viscosity Measurement 6.0
6.0
Relative Viscosity
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 71 %
71 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM DSC
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Users viewing this material also viewed the following: