Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ 5100 RD PBT; 15% Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved Surface. Property data for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
Flexural Yield Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 191 °C
376 °F
ASTM D648
Users viewing this material also viewed the following: