DSM Akulon® F-X9182 PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® F-X9182 PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low/Medium Viscosity
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
dry; ISO 1183
Viscosity 150000 cP

@Shear Rate 1000 1/s,
Temperature 290 °C
150000 cP

@Shear Rate 1000 1/s,
Temperature 554 °F
175000 cP

@Shear Rate 1000 1/s,
Temperature 260 °C
175000 cP

@Shear Rate 1000 1/s,
Temperature 500 °F
175000 cP

@Shear Rate 0.100 1/s,
Temperature 290 °C
175000 cP

@Shear Rate 0.100 1/s,
Temperature 554 °F
200000 cP

@Shear Rate 1000 1/s,
Temperature 230 °C
200000 cP

@Shear Rate 1000 1/s,
Temperature 446 °F
225000 cP

@Shear Rate 0.100 1/s,
Temperature 260 °C
225000 cP

@Shear Rate 0.100 1/s,
Temperature 500 °F
350000 cP

@Shear Rate 0.100 1/s,
Temperature 230 °C
350000 cP

@Shear Rate 0.100 1/s,
Temperature 446 °F
Viscosity Measurement 2.6
2.6
RSV formic acid, 1g/100ml; DSM method
Viscosity Test 160 cm³/g
160 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Thickness 50.0 microns
1.97 mil
film
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
dry; ISO 11359-1/-2
Descriptive Properties Value Comments
Extrusion Type Cast Film