Diamond Polymers DIAMALOY 1418 Polycarbonate/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 1418 Polycarbonate/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
ASTM D955
Melt Flow 6.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 4.6 %
4.6 %
chs 2.0 in/min; ASTM D638
Flexural Yield Strength 80.6 MPa
11700 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 2.139 GPa
310.2 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C

@Load 1.00 kg,
Thickness 3.17 mm
262 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1527