Diamond Polymers DIAMALOY PCPBT 530 PC/PBT Alloy, UV Stabilized/Weatherable

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY PCPBT 530 PC/PBT Alloy, UV Stabilized/Weatherable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
ASTM D955
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 265 °C
30 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.068 GPa
299.9 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 7.56 J/cm

@Thickness 3.17 mm
14.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 133 °C

@Load 1.00 kg,
Thickness 3.17 mm
271 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1527