Material Notes:
Acrylic adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of non-silicone coated substrates. Provides high temperature shear properties, excellent adhesion and solvent resistance.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Backing
38.1 microns
1.50 mil
Adhesive
Mechanical Properties Metric English Comments
Elongation at Break 130 %
130 %
Peel Strength 0.4602 kN/m
2.625 pli
Adhesion
6.14 kN/m
35.0 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
232 °C
450 °F
Intermittent
232 °C
450 °F
Shear Adhesive Failure (cohesive failure)
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Color Various
Users viewing this material also viewed the following: