Material Notes:
AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance clarity, sealability and toughness of the structure.Information provided by Dow
Physical Properties Metric English Comments
Density 0.868 g/cc
0.0314 lb/in³
ASTM D792
Mooney Viscosity 37

@Temperature 121 °C
37

@Temperature 250 °F
ML 1+4; ASTM D1646
Melt Flow 0.50 g/10 min
0.50 g/10 min
Melt Flow Ratio = 7.6 (I<sub>10</sub>/I<sub>2</sub>); ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
ASTM D2240
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D638
Tensile Strength, Yield 1.48 MPa
215 psi
ASTM D638
6.62 MPa
960 psi
100% Secant; ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 56.0 °C
133 °F
Dow Method
Vicat Softening Point <= 45.0 °C
<= 113 °F
ASTM D1525