Dow Corning 1-8114 SIH Crosslinker

Category Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 1-8114 SIH Crosslinker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Methylhydrogen terminated polydimethylsiloxane, 5cSt viscosity. 0.30%SiH. Molecular weight 562.Information provided by Dow Corning