Material Notes:
A blend of an ultrahigh viscosity polydimethylsiloxane in low viscosity polydimethylsiloxane for use in skincare, suncare, hair care, color cosmetic, and an antiperspirnt/deodorant applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 25.0 °C
0.900 g/cc

@Temperature 77.0 °F
Viscosity Measure 3300 cSt
3300 cSt
kinetic/kinematic
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.397
1.397
Descriptive Properties Value Comments
Active Content (%) 100
Cyclotetrasiloxane Content (max %) 0.94