Dow Corning 2-8203 SILICONE EMULSION

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-8203 SILICONE EMULSION.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning 2-8203 Emulsion is an amidofunctional siloxane microemulsion suitable to provide a "Fabric Care" benefit for rinse cycle fabric softeners. The use of this product provides softness, water absorbency, and ease of ironing when compared to conventional rinse cycle fabric softener compositions.Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 18 %
18 %
Particle Size 0.0050 µm
0.0050 µm
pH 4.5 - 6.5
4.5 - 6.5
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Non-Ionic yes
Water Absorbing yes