Information provided by Dow Corning
Physical Properties Metric English Comments
Solids Content 15 %
15 %
Volatiles 79.6 %
79.6 %
pH 4.0 - 6.0
4.0 - 6.0
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance colorless liquid
Color pale yellow
Non-Ionic yes