Material Notes:
Dow Corning® 37 Emulsion is a waterdilutable release agent. Containing 35 percent, 10,000 cs silicone fluid, Dow Corning 37 Emulsion: Offers excellent release of rubber, plastics and metals Will not carbonize or gum at mold temperatures Will not build up on molds Will not discolor molded parts Has good stability in either undiluted or diluted form Is compatible with other nonionic and anionic silicone emulsions, with glycerol, and with moderate concentrations of polyalkylene glycolsInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.997 g/cc

@Temperature 25.0 °C
0.997 g/cc

@Temperature 77.0 °F
Solids Content 35 %
35 %
pH 7.0
7.0
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Color white
Non-Ionic yes